Home >> News >> Turbo Mill for Silicon Oxide

Turbo Mill for Silicon Oxide

Publish: 2021-12-16 14:23:22

Views:

The people currently used in daily life are also more, the airflow pulverizer is smashed into the standard size, which is generally smashed into micrometers, usually our equipment is more The device is constructed, usually composed of a portion of a coarse, fine powder or a wind device, or the like. The main purpose is to use wind energy to be powdered, and have canceled the traditional screening at the time of use. The main application is more useful in many industries such as mining or building materials. Some industries such as metallurgical or building materials, chemicals, etc. are useful to use large crushers for work.

Turbo Mill for Silicon Oxide will rise during work, when the temperature of the working fluid is too high, the flow rate of the gas increases. Take air as an example, the critical speed at room temperature is 320 m / sec, when the temperature rises to 480 ° C, the critical speed can be increased to 500 m / sec, that is, the kinetic energy increases by 150%. Therefore, increasing the temperature of the working fluid is conducive to improving pulverization. The pressure of the working fluid is the main parameters of the jet speed, but also the main parameters affecting the fineness of the break. Typically, the higher the pressure of the working fluid, the faster the speed, the greater the kinetic energy.
When titanium powder is pulverized by superheated steam, the vapor pressure is usually 0.8 to 1.7 MPa, and generally pulverized calcined material is high, and the material after pulverized surface can be lower.

Alpa Quartz powder Turbo Mill for Silicon Oxide case share:

A mining company specializes in the development and production of stone-shaped sand, silicon fine powder,
company produces various models, various quality indicators Quartz sand and water washing stone sand is widely used in: glass and glass products, metallurgical manufacturing, cast steel, precision cast, furnace, refractory, ceramic glaze, ceramic billet, rubber, coating, etc. Guide, negotiate business!
Case parameters:
Product particle size: D100: 11.5μm
Hour Yield: 380kg

Daily maintenance of Turbo Mill for Silicon Oxide

1, during production It is necessary to check the temperature rise of the bearing frequently, when the temperature rise exceeds 50 ° C, should be closed, and the reason is to rule out the fault.
2, when the new machine is running, the drive belt is easy to elongate, and should pay attention to adjust the appropriate looseness of the belt to ensure the work life of the belt.
3, if the loss case should be checked frequently, replace the quality and production volume in time.
4, the blade, the bushing should often check the wear situation. If the wear is worn, the productivity is lowered, and the particle size is replaced after the particle size is replaced.
5, the host and the graded flow bearing are lipids, and the No. 2 special lipids are used 265-295. [123: 6The bearing temperature is too high.
7. The spiral feeder has been changed during the change of the lipid of 4,000 hours, and the calcium-based grease is added.


I hope everyone can buy the airflow crusher product for the heart!